Differential Scanning Calorimeter LDSC-A12
Labtron Differential Scanning Calorimeter offers a temperature range of -150 to 550°C, heating rates up to 80°C/min, and cooling rates up to 20°C/min. It features liquid nitrogen refrigeration cooling, 3 thermocouples for efficient operation, and is CE certified for quality assurance.